MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Petrothene® NA963083 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellent drawdown are needed. NA 963 exhibits uniformity, ease of processing and good tensile strength.

Regulatory Status
The basic resin NA 963 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.

Processing Techniques
Generally recommended extrusion conditions include a melt temperature range of 310°350°F; a blow-up ratio range of 1.8-2.5:1. Drawdown to 1.0 mils is possible at commercial rates when proper extrusion techniques are used. Specific recommendations for processing NA 963 can be made only when the end use applications, required properties and processing equipment are known.

Physical Properties
These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5" (98 mm)blown film line, commercially available 8"(203 mm) die, 350°F(177°C) melt extrusion temperature, 2:1 BUR, 1.25 mil(32 micron)gauge, 0.025" die gap at 150 lb/hr.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Thickness 31.8 microns1.25 mil2:1 BUR; 25 mil die gap
Melt Flow 0.70 g/10 min0.70 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646Molded; ASTM D2240
Tensile Strength at Break 11.4 MPa1650 psiMolded; ASTM D638
Tensile Strength, Yield 10.7 MPa1550 psiMolded; ASTM D638
Film Elongation at Break, MD 160 %160 %ASTM D882
Film Elongation at Break, TD 480 %480 %ASTM D882
Elongation at Break 700 %700 %Molded; ASTM D638
Elongation at Yield 100 %100 %Molded; ASTM D638
Elmendorf Tear Strength MD 300 g300 gASTM D1922
Elmendorf Tear Strength TD 180 g180 gASTM D1922
Dart Drop Test 130 g0.287 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 23.4 MPa3400 psiASTM D882
Film Tensile Strength at Break, TD 16.5 MPa2400 psiASTM D882
1% Secant Modulus, MD 179 MPa26000 psiASTM D882
1% Secant Modulus, TD 221 MPa32000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °FASTM D1525
Brittleness Temperature -75.0 °C-103 °FMolded; F50; ASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 °C350 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® NA963046 Low Density Polyethylene, Film Extrusion Grade
LyondellBasell Petrothene® NA960000 Low Density Polyethylene
LyondellBasell Alathon® L5440 High Density Polyethylene
LyondellBasell Petrothene® NA960083 Low Density Polyethylene
Chevron Phillips Marlex® 1122B Injection Molding Resin

PEQU0504 / 36971

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.