Onyx Elite® 103 is a high purity, organic free alumina trihydrate specifically designed to provide translucency, depth of pattern and soft white color polymer products. OE 103 is a high brightness alumina trihydrate featuring a unique particle size distribution which yields low resin demand and excellent air release properties.Information provided by J.M. Huber Corporation |