MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ChenGuang FPM 2602 Fluoroelastomer Copolymer Gum
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Molecular formula: -{(CH2CF2)0.8--[CF(CF3)CF2]0.2}n-

Properties:

  • Good heat resistance, solvent-resistance and excellent oil –resistance
  • Good physical and mechanical properties, good electrical insulation and anti-radiation properties

    Working under 250°C for long period, working at 300°C for short period

  • Low-temperature resistance not bad. Glass-transition temperature -17°C. Brittle point -40°C~-55°C
  • Not good resistance to low M.W. ketones, esters, some ethers, anhydrous ammonia and active amines.
Applications: Wildly used in aviation, automobile, petroleum, and chemical industries, mainly for sealing purpose. Especially good in the field of requiring heat-resistance and or oil-resistance. Usually be made into "O" sealing rings, "V" sealing rings, gasket, sealing bowl with metal bone. Suitable for both static and dynamic sealing of hydraulic and lubricating systems.

Storage: In shady cool and dry place.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 1.84 g/cc1.80 - 1.84 g/ccGum (before vulcanizing)
Viscosity 40 - 60 cP40 - 60 cPMooney, 2602 A
 50 - 70 cP50 - 70 cPMooney, 2602 B
 50 - 60 cP
@Temperature 121 °C
50 - 60 cP
@Temperature 250 °F
Mooney, 1+10, Gum (before vulcanizing)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 3.67 MPa>= 532 psibefore aging, Vulcanized Elastomer (without carbon black)
 >= 160 MPa>= 23200 psiafter aging, Vulcanized Elastomer (without carbon black)
Elongation at Break >= 150 %>= 150 %before aging, Vulcanized Elastomer (without carbon black)
Compression Set <= 55 %<= 55 %Vulcanized Elastomer (without carbon black)
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %Gum (before vulcanizing)
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 66 %66 %Gum (before vulcanizing)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU002 / 255601

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.