MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Johnson Matthey SIL-FOS® 6 6% Silver-Copper-Phosphorus Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Sil-fos™6 is used to braze copper and copper alloys. When brazing copper the phosphorus within the alloy imparts a metallurgical based self-fluxing capability. When Sil-fos™6 is used to join copper alloys (such as brass, bronze or gun metal) a separate flux will be required because the self-fluxing action only occurs on copper.

This filler metal should not be used to braze iron containing materials like carbon or stainless steels or nickel containing materials as the phosphorus within the filler metal will form brittle, intermetallic, phosphide compounds at the joint interface. Sil-fos™6 is not suitable for use in sulfurous atmospheres at elevated service temperatures.

When selecting a brazing filler metal from the Sil-fos™ range it is necessary to understand about the flow and ductility of the different products. Phosphorus is the key element, the higher this is the more free flowing the filler metal, but the lower its ductility. Silver is used to improve the filler metal’s ductility, but reduces its flow properties.

Sil-fos™6 is one of the most free flowing filler metals from the Sil-fos™ range. However, due to its high phosphorus content it is one of the least ductile. The low ductility of the alloy imparts it with glass like properties, making it both ‘notch’ sensitive and sensitive to impact type loadings. This filler metal should therefore not be used in applications involving exposure to strong vibration, impact loads or where some deformation of the joint might be expected in service. Sil-fos™6 is best suited for making copper joints that are of the true capillary type and where tight joint clearances of 0.025-0.075 mm are used. When used in such joints, the poor mechanical properties of the filler metal are exposed and satisfactory joints, suitable for use in all but the most extreme conditions can generally be produced.

Sil-fos™6 is extensively used in refrigeration and air conditioning applications for flux-free brazing of copper pipes and tubes. It is also used for joining copper in electrical engineering applications.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 644 - 718 °C
Solidus 644 °C
Liquidus 718 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 86.75 %
Phosphorus, P 7.25 %
Silver, Ag 6.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NJMMJ9751 / 186152

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.