MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Konson Calcium Stearate for PVC Heat Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical name: Calcium Stearate

CAS NO:1592-23-0

Molecular formula: Ca (C17H35COO) 2

Physical and Chemical Properties: white fine powder, nontoxic, soluble slightly in hot alcohol. It will absorb moisture in air and decompounds into stearate and calcium when meeting

Applications : Widely used as heat stabilizer for UPVC. It can increasing the gelation speed with base of lead salt and lead soap. Used as PP and PE halogen absorber to eliminates negative impact on residual catalyst to resin color and stability, improves resin’s yellow index and fluidity. Lubricant in polyolefin fiber and moulded work. Mold release, plasticizer, lubricating grease’s thickening agent, textile’s water proofing agent, paint flatting agent etc. for rubber processing. Used as good dispersing agent in color masterbatch, filler masterbatch. Used for food additives, forage additives and cosmetic etc.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 200 Mesh200 Mesh>98%
Molecular Weight 606 g/mol606 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 138 °C>= 280 °F
 
Component Elements PropertiesMetricEnglishComments
Calcium, Ca 6.4 - 6.8 %6.4 - 6.8 %
 
Descriptive Properties
Content<1%Free Acid (Stearic acid)
Loss of Drying<3%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS066 / 256111

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.