MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® PMMA 17OP Acrylic (Global)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: SABIC® PMMA 17OP is an optical LGP extrusion grade with low foreign matter count and low UV absorbance. The grade is available in pellet form.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccISO 1183
Water Absorption 0.30 %0.30 %24hr; ISO 62
Melt Flow 1.7 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.7 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9898ISO 2039
Tensile Strength, Yield 75.0 MPa10900 psiISO 527
Elongation at Yield 7.0 %7.0 %ISO 527
Modulus of Elasticity 3.30 GPa479 ksi1 mm/min; ISO 527
Flexural Strength 130 MPa18900 psiISO 178
Flexural Modulus 3.30 GPa479 ksi2 mm/min; ISO 178
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²ISO 179
Charpy Impact, Notched 0.160 J/cm²0.761 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
33.3 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FISO 75-1&2
Vicat Softening Point 101 °C214 °FB50; ISO 306
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491.49ISO 489
Haze 0.30 %0.30 %ISO 14782
Transmission, Visible 93 %93 %ISO 13468

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11130 / 244597

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.