MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Features: 15% Mineral Reinforced, Light Weight

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/cc(DAM); ASTM D792
Filler Content 15 %
Water Absorption 0.50 %24 hrs at 23°C (DAM); ASTM D570
Moisture Absorption at Equilibrium 2.1 %65% R.H. (from DAM); ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Thickness 1.00 mm
DAM
 0.014 - 0.018 cm/cm
@Thickness 3.00 mm
DAM
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPaASTM D638
 90.0 MPa
@Temperature -40.0 °C
ASTM D638
Tensile Strength, Ultimate 22.0 MPa
@Temperature 80.0 °C
ASTM D638
Flexural Strength 79.0 MPaASTM D790
 30.0 MPa
@Temperature 80.0 °C
ASTM D790
 152 MPa
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 2.30 GPaASTM D790
 1.40 GPa
@Temperature 80.0 °C
ASTM D790
 5.40 GPa
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched 60.0 J/m
@Temperature -40.0 °C
ASTM D256
 220 J/m
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmASTM D257
Dielectric Strength 21.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Arc Resistance 120 secASTM D495
Comparative Tracking Index >= 600 VIEC Method
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 290 °C(DAM)
Mold Temperature 50.0 - 120 °C(DAM)
Injection Pressure 50.0 MPa(DAM)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOY601 / 70761

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.