MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ovako 41Cr4 5515 Steel, Soft annealing
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: 41Cr4 is a steel for quenching and tempering recommended for components with strength requirements lower than the steel 42CrMo4. It is suitable for induction surface hardening, min hardness 52 HRC. It through hardens in oil up to appr. 40 mm diameter.

Information provided by Ovako

Key Words: 41CrS4, SS2245, 530M40, 530H40, EN18, SCR440, 42C4, 1.7035, 1.7039
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 241
@Thickness 20.0 - 160 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 320 °CMS
 735 °CAC1
 790 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.38 - 0.45 %
Chromium, Cr 0.90 - 1.2 %
Iron, Fe 96.99 - 98.1 %As Balance
Manganese, Mn 0.60 - 0.90 %
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.40 %
Sulfur, S 0.020 - 0.035 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovako 41Cr4 5515 Steel, Quench & Tempering
JIS S45C Steel, Normalized
CHT Group QM 254 60 Shore A, Addition Cure Moldmaking Material
AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
AISI 1010 Steel, CQ sheet,1.6-5.8 mm round or thickness

NOVAKO287 / 234586

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.