Clarified. Produced without animal derived components Sterilization: Gamma radiation, EtO, and E-beam Applications: Syringes, medical device components, labware Regulatory: FDA – 21 CFR 177.1520(c) 3.1a; USP <88> Class VI and ISO 10993-5 Information provided by INVISTA. |