MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik SIPERNAT® 310 Silica Powder
Categories: Other Engineering Material

Material Notes: Properties and applications: SIPERNAT represents a specific product range of precipitated silica, aluminum and calcium silicates. As a very finely ground silica with a very high surface area (BET), SIPERNAT 310 is used, for instant, as an antiblocking agent in polyolefins and PVC. Increase in color density and enhanced dot definition are benefits of this product applied as coating pigment for inkjet papers. It also can be used as binder or carrier in heterogeneous catalyst.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0950 g/cc0.00343 lb/in³Tamped; ISO 787-11
Particle Size 8.5 µm8.5 µmd50; ISO 13320-1
pH 6.06.05% in water; ISO 787-9
Specific Surface Area 700 m²/g700 m²/gISO 9277
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 97 %>= 97 %ISO 3262-19
Sodium, Na <= 1.0 %<= 1.0 %
 
Descriptive Properties
Content<1.5%Sulfate
 <400 ppmIron

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIM047 / 197251

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.