MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Multibase Multi-Flex® TPO 1047-4107
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Passed impact resistance 3.4J at -30°C; ASTM GM 9032 P. This product is UV stabilized for automotive applications, like fender guards and airbags.

Data provided by Multibase.

Key Words: Thermoplastic Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D792-91
Melt Flow 8.0 g/10 min8.0 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 424210 sec; ASTM D-2240-95
Tensile Strength, Ultimate 10.3 - 14.5 MPa1490 - 2100 psiASTM D638-95
Elongation at Break 500 - 700 %500 - 700 %ASTM D638-95
Flexural Strength 6.90 - 8.60 MPa1000 - 1250 psiASTM D790-95
Flexural Modulus, 1% Secant 213 - 255 MPa30900 - 37000 psiASTM D-790-95
Tear Strength Test 65 - 8865 - 88ASTM D624-95
 
Optical PropertiesMetricEnglishComments
Gloss 38 %38 %ASTM D2457-90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLA209 / 49606

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.