MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: WESTLAKE HIFOR Xtreme SC74838 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and medium antiblock. Films produced with this resin exhibit balanced toughness. Other features of this resin include good machine direction tear resistance.

    Application/Uses
  • Fresh produce packaging

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520.

All information provided by Westlake Chemical

Key Words: Balanced toughness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D1505
Thickness 25.4 microns1.00 mil
Melt Flow 1.0 g/10 min1.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 750 %750 %ASTM D882
Film Elongation at Break, TD 1000 %1000 %ASTM D882
Dart Drop 9.84 g/micron250 g/milASTM D1709
Film Tensile Strength at Break, MD 50.3 MPa7300 psiASTM D882
Film Tensile Strength at Break, TD 39.3 MPa5700 psiASTM D882
1% Secant Modulus, MD 200 MPa29000 psiASTM D882
1% Secant Modulus, TD 228 MPa33000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 13 %13 %ASTM D1003
Gloss 45 %45 %at 45º; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 216 °C400 - 420 °FBlown Film
Blow-up Ratio (BUR) 2.42.4As tested
 
Descriptive Properties
ProcessBlown Film
 Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake EB169 Low Density Polyethylene
ExxonMobil LLP8555.25 Rotational Molding Resin
Westlake LF2050 Hexene Linear Low Density Polyethylene
Westlake LF1050 Butene Linear Low Density Polyethylene
Westlake LF1040 Butene Linear Low Density Polyethylene

PWESF121 / 84558

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.