MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Hostacom 65F4-2 NATRL Polypropylene with 20% Talc Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Hostacom 65F4-2 NATRL conventional melt flow, 1,900 MPa flexural modulus, 20% talc-filled polypropylene homopolymer resin.  It has good impact resistance, dimensional stability, colorability and heat aging performance. Applications: Industrial.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inafter 48 hours at 23°C (tool); ASTM D955
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8484ASTM D785
Tensile Strength at Break 29.0 MPa4210 psiASTM D638
Tensile Strength, Yield 31.0 MPa4500 psiASTM D638
Elongation at Break 70 %70 %ASTM D638
Elongation at Yield 4.0 %4.0 %
Flexural Modulus 1.90 GPa276 ksiASTM D790
Izod Impact, Notched 0.370 J/cm
@Temperature 23.0 °C
0.693 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C228 °Funannealed; ASTM D648
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Matrixx 15A4201 Flame Retardant 20% Talc Filled Polypropylene (5VA)
A.D. Compound Adene NTFAG Copolymer 20% Talc Filled Polypropylene
LyondellBasell Astryn 65F4-2 Polypropylene Homopolymer, 20% Talc
LyondellBasell Hostacom 1202 3124 Polypropylene with 20% Talc Filler
LyondellBasell Hostacom 62F4-2C BLK P23431 Polypropylene with 20% Talc Filler

PEQT7644 / 219281

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.