  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Go Yen Chemical GOYENCHEM-TSH Foaming Agent-TSH
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 1576-35-8

Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC Group) is the most innovative manufacturer of fine CHEMICAL products in Taiwan with strong R&D team and abundant functional product lines. GOYENCHEM-TSH 4-Methylbenzenesulfonhydrazide (TSH) foaming agent can be widely used in intermediates, pharmaceutical and foaming agent of the world renown factories, that meet the requirements and can also improve products as well as its highly added value.

Advantages:

  • Especially suitable for the manufacture for closed-cell foam plastic and sponge rubber
  • Apply in polyvinyl chloride (PVC) for making white foam (mould need chrome plating)
  • Often used with sodium bicarbonate
  • Not suitable use with foaming agent H at the same time, in order to avoid too much heat, causing internal carbide
Applications:
  • Intermediates
  • Pharmaceutical
  • Plastic, natural and synthetic rubber foaming agent at low temperature
  • Can mixing below 70 ?
  • Generate the gas and decomposes the residue with nontoxic, odorless, free from contamination
  • Foam structure evenly and tightly
  • Small Product shrinking percentage
  • Good tear strength

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 105 - 108 °C221 - 226 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Descriptive Properties
Amount of Generating Gas120-130 ml/g
AppearanceWhite Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN358 / 266666

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.