Dexflex thermoplastic polyolefins (TPOs) are in use in applications once reserved for more expensive engineering resins. The performance of these TPOs, combined with their quality and consistency, makes them cost-effective alternatives in automotive applications. Dexflex E756-1 BLK is an unfilled PP TPO copolymer with excellent impact resistance. Applications: Interior Automotive Applications. Information provided by LyondellBasell. |