Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties. Key Features and Benefits: - Self adhesive resin system for sandwich panel applications
- Flame retardant and self-extinguishing
- Low tack and long out-times for ease of processing
Applications/Qualifications: - Sandwich panels / structures
- Aircraft Interiors
- Mass Transit Interiors
Information provided by Park Electrochemical Corp. |