MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® FR2375D LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: Formolene® FR2375D is a low density polyethylene with films exhibiting good mechanical and optical properties. Formolene® FR2375D is formulated without slip and antiblock for use in film applications offering excellent extrusion processing and very good balance of mechanical and optical properties.

Availability: North America

Additive: Antiblock: 450 ppm; Slip: 500 ppm

Features: Antiblocking; Excellent Processability; Good Optical Properties; Low Density; Slip

Uses: Agricultural Applications; Blending; Film; Laminates; Shrink Wrap

Form: Pellets

Processing Method: Coextrusion; Extrusion; Film Extrusion

Information provided by Formosa Plastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 450 ppm450 ppm
Slip Level 500 ppm500 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 310 %
@Thickness 0.0508 mm
310 %
@Thickness 0.00200 in
Blown Film; ASTM D882
Film Elongation at Break, TD 530 %
@Thickness 0.0508 mm
530 %
@Thickness 0.00200 in
Blown Film; ASTM D882
1% Secant Modulus  241 MPa
@Thickness 0.0508 mm
35000 psi
@Thickness 0.00200 in
MD, Blown Film; ASTM D882
 276 MPa
@Thickness 0.0508 mm
40000 psi
@Thickness 0.00200 in
TD, Blown Film; ASTM D882
Elmendorf Tear Strength MD 350 g
@Thickness 0.0508 mm
350 g
@Thickness 0.00200 in
Blown Film; ASTM D1922
Elmendorf Tear Strength TD 150 g
@Thickness 0.0508 mm
150 g
@Thickness 0.00200 in
Blown Film; ASTM D1922
Dart Drop Test 180 g
@Thickness 0.0508 mm
0.397 lb
@Thickness 0.00200 in
Blown Film; ASTM D1709
Film Tensile Strength at Break, MD 27.6 MPa
@Thickness 0.0508 mm
4000 psi
@Thickness 0.00200 in
Blown Film; ASTM D882
Film Tensile Strength at Break, TD 22.1 MPa
@Thickness 0.0508 mm
3200 psi
@Thickness 0.00200 in
Blown Film; ASTM D882
 
Optical PropertiesMetricEnglishComments
Gloss 59 %
@Thickness 0.0500 mm
59 %
@Thickness 0.00197 in
45°, Blown Film; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 190 °C356 - 374 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFPCR756 / 311449

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.