MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage cables. Specifications: IEC 60502 ISO 1872-E/BA, KHXY, 23-G200, C40

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.135 g/ccISO 1183/ISO 1872-2
Water Absorption 0.060 %Karl Fischer-titration
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break <= 2.20 MPaafter aging (168h, 135°C); IEC 60811-1-2
 11.0 MPa25mm/min; ISO 527
Elongation at Break 200 %25mm/min; ISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 100 ohm-cm
@Temperature 23.0 °C
DC; ISO 3915
 <= 1000 ohm-cm
@Temperature 90.0 °C
DC; ISO 3915
 
Processing PropertiesOriginal ValueComments
Melt Temperature 125 - 185 °C
Drying Temperature 60.0 °Chopper drying; 4h
Shelf Life 12.0 Month

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borlink™ LE7710 Polyethylene Compound, Semiconductive, Thermoplastic
Borealis Visico™ LE0540 Polyethylene Semiconductive Compound, Crosslinkable

PBOREA523 / 108782

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.