MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Oceanchem Group Calcium Bromide (CaBr2)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: CaBr2

Cas No.: 7789-41-5

Use: Calcium Bromide and its formuulated brines are mainly used as completion, workover and packer fluids in oil drilling field.

Properties: This product is white grain or cake crystal; it is free of smell and tastes salty and slightly bitter. It can dissolve in water and ethand or actone, hardly dissolves in aether or chloroform. It will turn yellow if placed in the air for a long time. It is very quick hygroscopic, its aqueous solution is neutral.

Storage and Handling: Product containers from damage and keep them well closed. Store in a cool, well-ventilated, dry and shaded storehouse. Avoid inhalation, ingestion and contact with the eyes and skin.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 - 1.73 g/cc0.0614 - 0.0625 lb/in³Liquid
pH 6.0 - 8.06.0 - 8.0Solid
 7.0 - 9.07.0 - 9.0Liquid
Molecular Weight 199.88 g/mol199.88 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 730 °C1350 °F
Boiling Point 806 - 812 °C1480 - 1490 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 3.0 %<= 3.0 %Solid
 
Descriptive Properties
AppearanceClear colorless to pack yellowLiquid
 White grain or lumpySolid
Assay (%)52Liquid; as CaBr2
 95Solid; as CaBr2
CAS Number7789-41-5
Chloride (%)<0.3Liquid
 <0.5Solid
Molecular FormulaCaBr2
Water-insoluble (%)<0.5Solid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POCEAN12 / 104216

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.