MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Mineral Filled

Material Notes: Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling

Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Low Warpage

Processing Method: Injection Molding

Forms: Pellets

Automotive Specifications: GM GMP.PA66.007

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D792
Water Absorption 0.80 %0.80 %24 hr; ASTM D750
Linear Mold Shrinkage 0.0070 - 0.012 cm/cm0.0070 - 0.012 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 89.6 MPa13000 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Elongation at Yield 1.8 %1.8 %ASTM D638
Flexural Strength 145 MPa21000 psiASTM D790
Flexural Modulus 6.55 GPa950 ksiASTM D790
Izod Impact, Notched 0.481 J/cm
@Temperature 22.8 °C
0.900 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 15.0 kV/mm
@Thickness 3.00 mm
380 kV/in
@Thickness 0.118 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.8 µm/m-°C26.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 202 °C395 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
Oxygen Index 27 %27 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 241 - 254 °C465 - 490 °F
Middle Barrel Temperature 257 - 274 °C495 - 525 °F
Front Barrel Temperature 263 - 282 °C505 - 540 °F
Nozzle Temperature 263 - 279 °C505 - 535 °F
Melt Temperature 257 °C495 °F
 263 - 279 °C505 - 535 °FProcessing Temperature
Mold Temperature 60.0 - 93.3 °C140 - 200 °F
Drying Temperature 79.4 °C175 °F
Moisture Content 0.20 %0.20 %
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Screw Speed 60 - 120 rpm60 - 120 rpm
 
Descriptive Properties
AppearanceBlack; Natural Color
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Chemlon® 140 M Nylon 66, 40% Mineral Reinforced

PTEKNO436 / 128613

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.