Description: Bales's application of .0002-.0003 Electroless Nickel with 10.5% to 12% phosphorus offers excellent corrosion protection against P.V.C. and other corrosive materials. Cores, cavities and entire mold bases can be coated with this engineering grade Electroless Nickel, offering a more uniform plated deposit than chrome. Information provided by Bales Mold Service Inc. |