MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Chemical Concepts Chem-Set™ CA100 General purpose adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: CA100 is a medium viscosity, rapid curing, cyanoacrylate adhesive. It is designed to bond a wide range of similar and dissimilar materials. Handling strength in most applications is in 10 seconds. Clear general purpose adhesive to bond a wide variety of dissimilar materials. Versatile offering good climatic, thermal and impact resistance. Handling strength 8 to 12 seconds. Mil Spec: MIL-A 46050 Type II Class I.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Viscosity 100 cP100 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 12.4 MPa>= 1800 psiISO 6922
Adhesive Bond Strength >= 5.17 MPa>= 750 psineoprene substrate, fixture time < 5 sec; ISO 4587
 >= 6.21 MPa>= 900 psiABS substrate, fixture time < 10 sec; ISO 4587
 >= 6.21 MPa>= 900 psiPVC substrate, fixture time < 5 sec; ISO 4587
 >= 6.21 MPa>= 900 psiPolycarbonate substrate, fixture time < 30 sec; ISO 4587
 >= 12.1 MPa>= 1750 psialuminum substrate, fixture time < 15 sec; ISO 4587
 >= 14.5 MPa>= 2100 psisteel substrate, fixture time < 20 sec; ISO 4587
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 - 1.00e+16 ohm-cm2.00e+15 - 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.0 - 3.5
@Frequency 1000 Hz
2.0 - 3.5
@Frequency 1000 Hz
ASTM D150
 
Descriptive Properties
Chemical CompositionCyanoacrylate adhesive
Chemical Resistance100% strength retained after aging 500 hrs in Ethanol @ 22°C
 100% strength retained after aging 500 hrs in Freon TA @ 22°C
 100% strength retained after aging 500 hrs in Gasoline @ 22°C
 100% strength retained after aging 500 hrs in Isopropanol @ 22°C
 100% strength retained after aging 500 hrs in Motor Oil @ 22°C
 100% strength retained after aging 500 hrs in Polycarbonate @ 40°C, @ 95% RH
Colorclear
Solvent BaseEthyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEMI935 / 232187

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.