MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
ASI® PS 54460 Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: MP 54460 is a medium viscosity epoxy/copolymer resin formulation recommended for industrial bonding, small potting and laminating applications where excellent structural, mechanical and electrical properties are required. This two-part adhesive exhibits good wetting, cures at room temperature and develops strong, low shrinkage bonds to most materials including optical fibers, glass ceramics, most metals and many rigid plastics. It has excellent dimensional stability over a wide temperature range. Fully cured MP 54460 is a durable electrical insulator with good physical properties, plus resistance to water, weather, ozone and oxygen, petroleum solvents, lubricating oils, jet fuels, gasoline, alcohol, salt solutions, mild acids and alkalis and many other organic and inorganic compounds.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
@Temperature 25.0 °C
part B
 1.12 g/cc
@Temperature 25.0 °C
mixed
 1.15 g/cc
@Temperature 25.0 °C
part A
Viscosity 40000 cP
@Temperature 25.0 °C
part A
 50000 cP
@Temperature 25.0 °C
mixed
 80000 cP
@Temperature 25.0 °C
part B
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 80
@Temperature 25.0 °C
Tensile Strength 6600 psi
Elongation at Break 2.35 %
@Temperature 25.0 °C
Adhesive Bond Strength 3700 psiLap Shear; 2024 T3 Aluminum Abraded / MEK Wipe
Peel Strength 25.0 pli
@Temperature 25.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 8.00e+14 ohm-cm
Dielectric Constant 4.5
@Frequency 100 Hz,
Temperature 25.0 °C
Dielectric Strength 440 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life >= 20.0 min
@Temperature 25.0 °C
50 grams
Shelf Life 12.0 Month
 
Descriptive Properties
Color / appearanceoff white
Mix Ratio2:1 (by volume. Part A to Part B)
 213 : 100 (by weight. Part A to Part B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9094 / 233461

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.