MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Matexcel BIOD-003 PCL Electrospinning Microspheres
Categories: Wood and Natural Products

Material Notes: BIOD-003; PCL Electrospinning Microspheres; biodegradable material; Biopolymer materials

Application: The microsphere product can simulate the nanofibrous structure of natural extracellular matrix, promote the interaction between cells and matrix, and then promote cell adhesion, proliferation and differentiation. Widely used in cell culture, drug controlled release, tissue engineering and other fields.

Morphology: Fibrous porous microspheres

Key Words: Synonyms: PCL Electrospinning Microspheres
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 100 - 300 µm100 - 300 µm
Storage Temperature 4.00 °C39.2 °F
 
Descriptive Properties
Product overviewThis product is a nanofiber microsphere prepared by combining biodegradable polymer materials and micro-nano processing technologies such as electrospinning. Combines the functional advantages of nanofibers and microspheres. The product has high porosity, high specific surface area and good mechanical properties.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1973 / 300604

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.