Paper reinforcement, Phenolic Resin, Natural Color. High mechanical strength. Electrical properties are secondary. Applications - Superstructure support pads
- Bus bar insulators
- Pot cradle insulators
- Exhaust duct insulators
- Machined parts
- Wedges & shunts
- Point feeder gaskets
Advantages - High insulation properties
- High strength
- Low moisture absorption
- High temperature resistance
Information provided by Pyrotek. |