MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Sirmax Dafnetherm® PP GR16 PP, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Carbon Fiber Filled

Material Notes: Crystalline carbon filled polypropylene homopolymer. Thermally and electrically conductive.

Application: Injection Molding

Information provided by Sirmax®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.66 - 1.68 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.0 MPa5 mm/min; ISO 527-2
Elongation at Break 0.50 %5 mm/min; ISO 527-2
Tensile Modulus 8500 MPa2 mm/min; ISO 527-2
Izod Impact, Notched (ISO) 1.00 kJ/m²ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1000 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 3.00 W/m-Kin-plane; ISO 22007-2
 10.0 W/m-Kthrough-plane; ISO 22007-2
Vicat Softening Point 130 °CB50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °CISO 294
Mold Temperature 60.0 - 80.0 °CISO 294
Drying Temperature 80.0 - 90.0 °C
Dry Time 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIRMX034 / 281137

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.