Hifax CB 1160 G1 is a talc filled PP copolymer, with medium flowability, high impact resistance and good stiffness. This grade is delivered in customer customized colors. This Data Sheet is giving general properties, some of them may be slightly altered upon color selected. Status: Commercial - Active Availability: Europe Application: Bumpers; Exterior Trim Market: Automotive Processing Method: Injection Molding Attribute: Good Stiffness; High Impact Resistance; Medium Flow Information provided by LyondellBasell. |