MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Konson CBS-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80% N-cyclohexyl-2-benzothiazyl sulphenamide based on specification, 20% EPDM binder and dispersing agents

Use Characteristics: The curing accelerator Konson® CBS-80 provides a considerably long scorch time, great processing safety and a fast full cure. Konson® CBS-80 is used as a sole accelerator for the low sulphur vulcanization or in combination with dithiocarbamate or thiuram accelerators. The vulcanizates obtained have good ageing resistance and a good compression set. The scorch time of compounds containing Konson® CBS-80 in combination with thiurams and dithiocarbamates is noticeably reduced. Thiourea has a strong secondary acceleration effect on Konson®CBS-80, mainly in mixes containing little sulphur. In compounds which are accelerated with mercaptanes and thiu-rams, Konson® CBS-80 may delay scorch

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easy quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective CBS is assured.

Dosage levels: NR: primary: 0.5 – 1.0 phr with 2.5 – 3.5 phr sulphur secondary: 0.5 phr with 1.5-3.0 phr sulphur and 0.3 phr mercapto or thiuram accelerators SBR: 1.0 – 1.4 phr with 1.5 – 2.5 phr sulphur and 0 – 0.2 phr thiuram accelerator

Applications: Automotive and construction profile, Tire treads, air hoses, conveyor belts, footwear and other technical articles.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³
Ash <= 0.40 %<= 0.40 %
Evaporation Loss <= 0.50 %<= 0.50 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 96.0 °C205 °F
 
Descriptive Properties
AppearanceGrey-white or light-yellow granules
Content= 1.0 %Free amine
 = 94 %CBS
Insoluble= 0.4 %in ethanol
Sieve residue= 0.1 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS027 / 256072

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.