CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used in high temperature applications. CENTROTRON has a low sliding friction coefficient and high abrasion resistant. Applications include bearings, sealing rings, rods and hollow bars. Information provided by CENTROPLAST Engineering Plastics GMBH |