MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 1199-H18
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 1000 Series Aluminum

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
The aluminum content for unalloyed aluminum made by a refining process is the difference between 100.00 percent and the sum of all other metallic elements present in amounts of 0.0010 percent of more each, expressed to the third decimal before determining the sum, which is rounded to the second decimal before subtracting. When an element's specified maximum limit is 0.0XX, an observed value or a calculated value greater than 0.0005 but less than 0.0010% is rounded off and shown as " less than 0.001 ".
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 1199-H18; Refined Aluminum; Refined Aluminium; Raffinal; Super-purity Aluminum; UNS A91199, AA1199-H18; Al1199-H18
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 31500 kg load with 10 mm ball. Calculated value.
Tensile Strength, Ultimate 115 MPa
Tensile Strength, Yield 110 MPa
Elongation at Break 5.0 %
@Thickness 1.60 mm
In 5 cm
Tensile Modulus 62.0 GPaCompressive Modulus is about 2% higher
Poissons Ratio 0.33
Shear Modulus 25.0 GPa
Shear Strength 74.0 MPaCalculated value.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000280 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 390 J/g
CTE, linear 21.8 µm/m-°C
@Temperature -50.0 - 20.0 °C
 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
 24.5 µm/m-°C
@Temperature 20.0 - 200 °C
 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.900 J/g-°C
Thermal Conductivity 240 W/m-K
Melting Point 660 - 660 °C
Solidus 660 °C
Liquidus 660 °C
 
Optical PropertiesOriginal ValueComments
Reflection Coefficient, Visible (0-1) 0.87
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al >= 99.99 %Specified
Copper, Cu <= 0.006 %
Gallium, Ga <= 0.005 %
Iron, Fe <= 0.006 %
Magnesium, Mg <= 0.006 %
Manganese, Mn <= 0.002 %
Other, each <= 0.002 %
Silicon, Si <= 0.006 %
Titanium, Ti <= 0.002 %
Vanadium, V <= 0.005 %
Zinc, Zn <= 0.006 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 1199-O
Aluminum 1050-H14
Aluminum 1180-H18
Aluminum 1180-O
Aluminum 1145-O

MA1199H18 / 8778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.