MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta EndurX™ BP21NPM Phenolic Cotton Laminate Sheet, MoS2 Lubricated
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: BP21NPM is composed of a linen substrate combined with a phenolic resin system which contains molybdenum disulfide for reduced wear and increased lubrication. Provides the same lubricity as BP13NPM, but has better machining qualities. The mechanical strength is similar to, but slightly less than BP21NPN. BP21NPM is used in applications where reduced wear is needed in non-conductive applications.

Key Words: Cotton, Phenolic, Micarta, Molybdenum Disulfide Lubricant
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/ccASTM D792
Moisture Absorption 2.40 %
@Time 86400 sec
2.40 %
@Time 24.0 hour
Condition D1-24/23; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 103103ASTM D785
Tensile Strength  66.9 MPa
@Thickness 3.17 mm
9700 psi
@Thickness 0.125 in
Condition A, Crosswise; ASTM D638
 96.5 MPa
@Thickness 3.17 mm
14000 psi
@Thickness 0.125 in
Condition A, Lengthwise; ASTM D638
Flexural Strength  124 MPa
@Thickness 1.57 mm
18000 psi
@Thickness 0.0620 in
Condition A, Crosswise; ASTM D790
 164 MPa
@Thickness 1.57 mm
23800 psi
@Thickness 0.0620 in
Condition A, Lengthwise; ASTM D790
Flexural Modulus  7.58 GPa
@Thickness 1.57 mm
1100 ksi
@Thickness 0.0620 in
Condition A, Crosswise; ASTM D790
 10.3 GPa
@Thickness 1.57 mm
1500 ksi
@Thickness 0.0620 in
Condition A, Lengthwise; ASTM D790
Compressive Strength 269 MPa
@Thickness 12.7 mm
39000 psi
@Thickness 0.500 in
Condition A, Flatwise; ASTM D695
Shear Strength 100 MPa
@Thickness 1.57 mm
14500 psi
@Thickness 0.0620 in
Condition A, Perpendicular; ASTM D732
Adhesive Bond Strength 13.1 MPa
@Thickness 12.7 mm
1900 psi
@Thickness 0.500 in
Condition A, Bonding Strength; ASTM D229
Izod Impact, Notched  0.694 J/cm
@Thickness 12.7 mm
1.30 ft-lb/in
@Thickness 0.500 in
Condition E-48/50, Crosswise; ASTM D256
 0.854 J/cm
@Thickness 12.7 mm
1.60 ft-lb/in
@Thickness 0.500 in
Condition E-48/50, Lengthwise; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown  5000 V
@Thickness 1.57 mm
5000 V
@Thickness 0.0620 in
Condition D-48/50; ASTM D149
 30000 V
@Thickness 1.57 mm
30000 V
@Thickness 0.0620 in
Condition A; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.0 µm/m-°C
@Thickness 3.17 mm
5.56 µin/in-°F
@Thickness 0.125 in
X-axis; IPC-TM 650-2.4.24
 12.0 µm/m-°C
@Thickness 3.17 mm
6.67 µin/in-°F
@Thickness 0.125 in
Y-axis; IPC-TM 650-2.4.24
UL RTI, Electrical 130 °C266 °FUL Bulletin 746b
UL RTI, Mechanical without Impact 130 °C266 °FUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0620 in
Condition A
 
Descriptive Properties
SubstrateCotton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNORPM235 / 280551

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.