Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU). Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency and UV stability. Uses: Extrusion: Hose and Tube, Profile, Cable Jacket. Injection molding: Various. Available in Americas, Europe, Middle East, Africa, India and Asia Information Provided by The Lubrizol Corporation |