MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ensinger TECACOMP PPS TRM XS black 1014938 PPS, Carbon Fiber Reinforced, Solid Lubricant Filled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler

Material Notes:
  • very good bearing and wear properties
Target Industries:
  • automotive industry
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors: Ensinger TECACOMP compounds withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Bulk Density 0.550 g/ccEN ISO 60
Density 1.47 g/cc
Water Absorption at Saturation <= 0.10 %50 % relative humidity up to saturation; DIN EN ISO 62
Linear Mold Shrinkage, Flow 0.0013 cm/cmDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0064 cm/cmDIN EN ISO 294-4
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 316 °C
DIN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 135 MPa50 mm/min; DIN EN ISO 527-1
Elongation at Break 0.50 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 22.5 GPa50 mm/min; DIN EN ISO 527-1
Charpy Impact Unnotched 18.0 kJ/m²DIN EN ISO 179-1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6200 ohm-cmDIN EN ISO 3915
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 9.00 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN EN ISO 11359-1;2
CTE, linear, Transverse to Flow 47.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN EN ISO 11359-1;2
Thermal Conductivity 0.700 W/m-Kthrough-plane; ISO 22007-4:2008
 1.10 W/m-Kin-plane; ISO 22007-4:2008
Melting Point 280 °CDIN 53765
Maximum Service Temperature, Air 230 °Clong term
 260 °Cshort term
Deflection Temperature at 0.46 MPa (66 psi) 285 °CISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 280 °CISO-R 75 Method A
Glass Transition Temp, Tg 90.0 °CDIN 53765
Flammability, UL94 V-0DIN IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Processing Temperature 300 - 350 °CCylinder
Melt Temperature 335 - 360 °CMaterial temperature
Mold Temperature 140 - 160 °C
Drying Temperature 140 - 150 °C
Dry Time 4.00 - 6.00 hour
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIO9128 / 319056

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.