MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chi Mei Kibilac® PW-997L ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Product Description: Matting ASA features and benefits: Excellent weatherability; colorfastness for outstanding exterior design; matting characteristic increases housing aesthetics

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Good Color Stability; Good Weather Resistance

Uses: Housings; Outdoor Applications

RoSH Compliance: RoSH Compliant

Appearance: Matte Finish

Information provided by Chi Mei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 44.1 MPa6400 psi0.24 in/min; ASTM D638
Elongation at Break 35 %35 %0.24 in/min; ASTM D638
Flexural Strength 68.7 MPa9960 psi0.11 in/min; ISO 178
Flexural Modulus 2.21 GPa320 ksi0.11 in/min; ISO 178
Izod Impact, Notched 0.801 J/cm
@Thickness 3.17 mm
1.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
@Thickness 6.35 mm
185 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 110 °C230 °FRate A (50°C/h), Loading 1 (10 N); ASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 20 %20 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHJ353 / 311046

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.