MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Silvaloy® B72 Brazing Alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy B72 is the eutectic composition of the silver-copper system. It is suitable for use in controlled atmosphere brazing without the use of a paste flux. When molten, it is very fluid and may flow out over the work surfaces during some furnace brazing applications. The wetting action on ferrous metals is limited, minimizing its use on carbon steel. Improved wetting is observed when furnace brazing of stainless steel with silver-copper filler metals. Most applications for this alloys are on copper and nickel base alloys. Typical applications are the joining of ferrous, nonferrous, and dissimilar metals and alloys with close joint clearances.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Key Words: AWS BAg-8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 9.06 g/cc9.06 g/cc
Density 9.96 g/cc0.360 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 ohm-cm0.00000200 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 779.4 °C1435 °F
Solidus 779.4 °C1435 °F
Liquidus 779.4 °C1435 °F
Maximum Service Temperature, Air 204 °C400 °Fcontinuous
 316 °C600 °Fintermittent
 
Processing PropertiesMetricEnglishComments
Processing Temperature 779.4 - 899 °C1435 - 1650 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 26.85 - 29 %26.85 - 29 %As balance
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 71 - 73 %71 - 73 %
 
Descriptive Properties
ColorWhite
Electrical Conductivity (% IACS)87

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Silvaloy® A56T Brazing Alloy
Cadi 50WS Tungsten Silver
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Lucas-Milhaupt Silvaloy® 501 Brazing Alloy
Lucas-Milhaupt Silvaloy® A56T Flux Coated Rod Brazing Alloy

NBRW046 / 79822

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.