MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MetalTek MTEK 6XN Cast UNS J94651 Super Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; Cast Stainless Steel

Material Notes: Corrosion resistance approaching nickel alloys, especially in chloride service.

Applications: Process piping exposed to flue gas and solutions.

Information provided by MetalTek

Key Words: Cast UNS J94651; Cast Grade CN3MN; Cast ASTM A743, A744; Wrought UNS N08367; Wrought Grade AL6XN®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 550 MPa
Tensile Strength, Yield >= 260 MPa
Elongation at Break >= 35 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 20 - 22 %
Iron, Fe 42.21 - 50.32 %As Balance
Manganese, Mn <= 2.0 %
Molybdenum, Mo 6.0 - 7.0 %
Nickel, Ni 23.5 - 25.5 %
Nitrogen, N 0.18 - 0.26 %
Silicon, Si <= 1.0 %
 
Descriptive Properties
Heat TreatmentSol. Anneal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek MTEK 2507 Cast UNS J93404 Duplex Stainless Steel
MetalTek MTEK 20 Cast UNS N08007 Super Austenitic Stainless Steel
MetalTek MTEK CW-12MW Cast UNS N30002 Severe Corrosion and Heat Resistant Alloy
ASTM A439 Austenitic Ductile Iron type D2
AISI Type T15 Tungsten High Speed Tool Steel (UNS T12015)

NMETEK058 / 18308

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.