MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: 250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.

Kapton® Type HN film coated with Teflon® FEP fluoropolymer resin, imparts heat sealability, provides a moisture barrier, and enhances chemical resistance.

General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianhydride with an aromatic diamine. It has excellent chemical resistance; there are no known organic solvents for the film. It does not melt. It can be used at both high and low temperature extremes. Kapton® polyimide films can be used in a variety of electrical and electronic uses: wire and cable tapes, formed coil insulation, substrates for printed circuit boards, motor slot liners, magnet wire insulation, transformer and capacitor insulation, magnetic and pressure-sensitive tapes, and tubing.

Data provided by DuPont High Performance Films.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ASTM D542-90
Moisture Absorption at Equilibrium 0.40 %0.40 %50% RH; 23°C (400=FN022)
 1.2 %1.2 %98% RH; 23°C
Water Vapor Transmission 2.40 g/m²/day0.155 g/100 in²/day
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD  36.0 MPa
@Temperature 200 °C
5220 psi
@Temperature 392 °F
3% yield point; Orientation not specified; ASTM D882-91
 58.0 MPa
@Temperature 23.0 °C
8410 psi
@Temperature 73.4 °F
3% yield point; Orientation not specified; ASTM D882-91
Film Elongation at Break, MD 85 %85 %Orientation not specified. Value at 200°C (390°F) is 110%; ASTM D882
Secant Modulus  1.38 GPa
@Temperature 200 °C
200 ksi
@Temperature 392 °F
ASTM D882
 2.62 GPa
@Temperature 23.0 °C
380 ksi
@Temperature 73.4 °F
ASTM D882
Impact Test 1.56 J1.15 ft-lbImpact strength per DuPont Pneumatic Impact Test
Tear Strength Test 17.817.8N Graves (Initial) value; ASTM D1004-90
Elmendorf Tear Strength MD 58 g58 gOrientation not specified; ASTM D1922-89
Film Tensile Strength at Break, MD 200 MPa29000 psiOrientation not specified; ASTM D882
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.90e+17 ohm-cm1.90e+17 ohm-cm
Dielectric Constant 3.03.0
Dielectric Strength 197 kV/mm5000 kV/in
Dissipation Factor 0.00130.0013
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.09 J/g-°C0.261 BTU/lb-°FValue for Kapton® HN
Thermal Conductivity 0.120 W/m-K0.833 BTU-in/hr-ft²-°FValue for Kapton® HN
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film
DuPont™ Kapton® 150FN019 Polyimide/FEP Composite Film
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
Westlake Plastics TPX® Polymethylpentene
DuPont™ Kapton® 500FPC Polyimide Film, 125 Micron Thickness

PDUK33 / 33403

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.