MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SCG Chemicals EL-Lene™ M3504DXP Octene (C8) Rotational Molding Resin
Categories: Polymer; Thermoplastic

Material Notes: Natural base resin available in powder form

Key Characteristics:

  • Excellent ESCR
  • Excellent impact resistance
  • Low warpage
  • Fair processing

Typical Applications: Chemical storage tanks, diesel tanks, spray tanks, IBC, and marine products

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.935 g/cc0.935 g/ccASTM D1505
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psiASTM D638
Elongation at Break 1100 %1100 %ASTM D368
Flexural Modulus 0.650 GPa94.3 ksiASTM D790
Dart Drop Total Energy 2.30 J/cm
@Thickness 5.00 mm,
Temperature -40.0 °C
0.00431 ft-lb/mil
@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FASTM D2117
Crystallization Temperature 105 °C221 °FASTM D2117
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact; FDA and AS/NZS 4020
 
Descriptive Properties
Heavy Metal Free (Base Resin)Yes
Peak Internal Air Temperature225°CTPE Method
Shrinkage Levelvery smallTPE Method
UV StabilizerUV-6 &UV-8ASTM G155

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC937 / 120691

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.