MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Reynolds Ecoflex™ 00-45 Near Clear™ Super-Soft, Exceptionally Clear Silicone Rubbers
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Product Overview: Ecoflex™ Near Clear™ rubbers are very soft, platinum silicones that are clearer than other Ecoflex™ silicones. Versatile and easy to use, Ecoflex™ Near Clear™ rubbers are mixed 1A:1B by weight or volume and cure at room temperature with negligible shrinkage. Low viscosity ensures easy mixing and de-airing. Ecoflex™ Near Clear™ silicones are available in Shore 00-31 and Shore 00-45 hardness formulations. Cured material is skin safe and certified by an independent laboratory. Cured rubber is very soft, very strong and very “stretchy”, stretching many times its original size without tearing and will rebound to its original form without distortion. Ecoflex™ Near Clear™ rubbers can be color pigmented with Silc Pig™ pigments, Cast Magic™ powders or Glow Worm™ powders for creating a variety of color effects. You can also add Smooth-On’s Silicone Thinner™ to further lower the viscosity

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D-1475
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 4545ASTM D-2240
Tensile Strength 2.17 MPa315 psiASTM D-412
Elongation at Break 980 %980 %ASTM D-412
100% Modulus 0.0827 MPa12.0 psiASTM D-412
Tear Strength 8.77 kN/m50.0 pliDie B; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min4.00 hour
Pot Life 45.0 min45.0 minASTM D-2471
 
Descriptive Properties
ColorWater Clear Translucent
Mix Ratio1A:1Bby volume or weight
Specific Volume26.2[in3/lb]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN332 / 297033

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.