MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Barlog Plastics KEBABLEND M 17/22 PA6 for Plastic Bonded Magnets
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: PA6 functional compound for the production of plastic bonded magnets

Properties: magnetizable

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.73 g/cc0.135 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psiISO 527-1
Elongation at Break 0.800 %0.800 %ISO 527-1
Modulus of Elasticity 22.0 GPa3190 ksiISO 527-1
 
Electrical PropertiesMetricEnglishComments
Magnetic Coercive Force, Hc 2765 Oe2765 Oe220 kA/m; DIN EN 60404-5
Magnetic Remanence, Br 2950 Gauss2950 Gauss295 mT; DIN EN 60404-5
Magnetic Maximum Energy Product, BH 2.14 MGOe2.14 MGOe17 kJ/m³; DIN EN 60404-5
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357-1/-3
Flammability, UL94  HB
@Thickness 0.400 mm
HB
@Thickness 0.0157 in
IEC 60695-11-10
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 310 °C536 - 590 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
Back Pressure 4.00 - 8.00 MPa580 - 1160 psi
 
Descriptive Properties
Magnetic properties17 kJ/m³max. energy product (BH max), DIN EN 60404-5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO431 / 326505

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.