MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Nylatron™ / Ertalon™ LFX PA6 Lubricated Cast PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: A self-lubricating cast nylon 6 that displays strong mechanical strength, great sliding properties, high mechanical damping capabilities, and exceptional electrical insulating properties.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 82.0ASTM D785
Hardness, Shore D 76.0ISO 868
Tensile Strength 73.0 MPaISO 527-1/-2 (7)
Elongation at Yield 5.00 %ISO 527-1/-2 (7)
Flexural Strength 107 MPaISO 178 (12)
Compressive Yield Strength 31.0 MPa
@Strain 1.00 %
ISO 604 (10)
 58.0 MPa
@Strain 2.00 %
ISO 604 (10)
 85.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 4.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 22.0 kV/mmIEC 60243-1 (15)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.280 W/m-K
Minimum Service Temperature, Air -20.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ 66 SA PA66 AE Polyamide 66, extruded
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Mitsubishi Chemical Advanced Materials Nylatron™ / Ertalon™ 4.6 PA4.6 PA 4.6, extruded
Mitsubishi Chemical Advanced Materials Nylatron™ GF30 / Ertalon™ 66 GF30 PA66 30% glass filled, extruded

P1SMU836 / 130658

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.