Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonable pricing. DIAMAT® utilizes acrylic toughener technology resulting in consistent appearance, even after years of UV exposure. DIAMAT® IG is an acrylic molding resin for injection molding, with well balance impact strength and heat resistance. Information provided by US distributor, API-Kolon. |