MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Nouryon Eka HP C (Chemical Grade) Hydrogen Peroxide
Categories: Other Engineering Material

Material Notes: Eka HP C (Chemical Grade) hydrogen peroxide solutions are clear, colorless and water-like in appearance. They are available in a number of different concentrations. Please contact your Nouryon Representative to determine which product meets your requirements. your Nouryon Representative to determine which product meets your requirements.

CAS number: 7722-84-1

Molecular formula: H2O2

Applications: This grade is our highest purity and is designed to meet the stringent demands of customers in chemical and metal processing applications and the electronics industry. In the chemical industry, hydrogen peroxide plays a major role in the production of both inorganic and organic products. Examples include the manufacturing of percarbonates, perborate, a wide variety of organic peroxides and propylene oxide. Hydrogen peroxide is a mainstay in surface treatment within the metals and electronics industry; it is used for etching, polishing and cleaning, plus it eliminates nitrogen oxide gases (NOx) in connection with nitric acid-based pickling operations. Hydrogen peroxide is also used as a reducing agent in the production of chlorine dioxide – a bleaching agent used in the pulp industry.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 34.02 g/mol34.02 g/mol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY503 / 286026

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.