MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Humiseal 1B12 Acrylic Conformal Coating
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Humiseal 1B12 Acrylic Conformal Coating
  • High moisture resistance
  • Excellent dielectrical properties
  • Selective chemical resistance
  • Excellent repairability
  • Passes thermal shock test (MIL-I-46058C)
  • Flammability (self extinguishing) (ASTM D635)
  • Poor resistance to solvents (IPC CC 830)
  • Recommended Stripper: 1080
  • Recommended Thinner: 503/521
Cure Type: Room Temp or Heat

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.30 lb/galASTM D1475
Solids Content 20 %Fed Std 141 Method 4044
Volatile Organic Compounds (VOC) Content 701 g/l
Viscosity 40 cPFed Std Method 4287
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 9.782 ksi
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 3.00e+10 ohmMoisture Resistance; MIL-I-46058C
Insulation Resistance 2.50e+14 ohmInsulation Resistance; MIL-I-46058C
Dielectric Constant 2.8ASTM D1 50 65T
Dielectric Breakdown >= 1500 VDielectric Withstand; MIL-I-46058C
Dissipation Factor 0.010ASTM D1 50 65T
 
Thermal PropertiesOriginal ValueComments
CTE, linear 56.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -65.0 °C
Glass Transition Temp, Tg 32.0 °C
Flash Point 30.0 °FASTM D56
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 minDry Time to Handling; Fed Std 141 4061
 0.500 hour
@Temperature 170 °C
 >= 24.0 hour
@Temperature 23.0 °C
Shelf Life 12.0 Month
@Temperature 23.0 °C
 
Descriptive Properties
Coverage330 ft²/gal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® Output™ 315 Acrylic Adhesive
Parson Adhesives PARTITE® 9326 Acrylic Structural Adhesive
Humiseal 1B31 Acrylic Conformal Coating
Henkel Loctite® Output™ 383 Acrylic Adhesive
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP

PHUMIS00 / 47600

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.