System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Malleable iron casting, Class M4504 air quenched and tempered
Categories:
Metal
;
Ferrous Metal
;
Cast Iron
;
Malleable Iron
Material Notes:
Automotive. Ferritic and tempered pearlite, may be tempered martensite for some applications. Applications include compressor crankshafts and hubs.
Key Words:
ASTM A602, SAE J158, Malleable iron casting grade M4504, automotive, ferritic, good machinability
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Original Value
Comments
Hardness, Brinell
163 - 217
Hardness, Knoop
211
Estimated from Brinell
Hardness, Vickers
199
Estimated from Brinell
Tensile Strength, Ultimate
448
MPa
Tensile Strength, Yield
310
MPa
Elongation at Break
4.0 %
Component Elements Properties
Original Value
Comments
Carbon, C
2.45 - 2.55 %
Chromium, Cr
0.040 - 0.070 %
Copper, Cu
0.030 - 0.40 %
Iron, Fe
94.4 - 95.6 %
As Balance
Manganese, Mn
0.35 - 0.55 %
Molybdenum, Mo
0.030 - 0.10 %
Nickel, Ni
0.050 - 0.30 %
Phosphorus, P
<= 0.030 %
Silicon, Si
1.4 - 1.5 %
Sulfur, S
0.050 - 0.070 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
ASTM A197 malleable iron casting
Malleable iron casting, Class M5503 liquid quenched and tempered
ASTM class 30 Standard gray iron test bars, as cast
Malleable iron casting, Class M3210 annealed
Ductile Iron grade 60-40-18
MMFE13 / 12435
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.