MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

RAMPF RAKU® TOOL EH-2982 Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Properties:
  • Rapid to medium setting, adjustable pot life
  • 1:1 resin to hardener ratio by weight or volume
  • Color indicator for easy mixing
  • Transparent bond line after curing
  • No special handling or application techniques
Applications:
  • Small part bonding
  • Rapid repair
  • Bonding tooling boards
  • Bonding metal, glass, wood, most rigid plastics, concrete, stones
  • Not recommended for polyolefins, Teflon, Nylon or flexible materials
Cure: 2 days at 25°C

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
 1.15 g/cc0.0415 lb/in³EA-2800 / EH-2982, cured; ISO 1183
Viscosity 10000 - 15000 cP10000 - 15000 cPEA-2800 / EH-2982; ISO 2555
 10000 - 15000 cP10000 - 15000 cPISO 2555
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 8580 - 85EA-2800 / EH-2982, cured; ISO 868
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 - 2880 min24.0 - 48.0 hourEA-2800 / EH-2982, Minimum curing time
Pot Life 3.00 - 4.00 min3.00 - 4.00 minEA-2800 / EH-2982, 100 ml
 
Descriptive Properties
AspectTransparentEA-2800 / EH-2982
ColorPale Yellow
Mix Ratio100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF003 / 317603

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.