SABIC LEXAN™ 121M PC (Americas)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
Non-halogenated. 17.5 MFR, for small, intricate parts. Improved internal mold release. ...
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.20
g/cc
1.20
g/cc
ASTM D792
1.20
g/cc
1.20
g/cc
ASTM D792
Density
1.19
g/cc
0.0430
lb/in³
ASTM D792
Water Absorption
0.15 %
0.15 %
24 hours; ASTM D570
Moisture Absorption at Equilibrium
0.35 %
0.35 %
ASTM D570
0.58 %
@Temperature 100 °C
0.58 %
@Temperature 212 °F
ASTM D570
Linear Mold Shrinkage, Flow
0.0050
-
0.0080
cm/cm
@Thickness 3.20 mm
0.0050
-
0.0080
in/in
@Thickness 0.126 in
SABIC method
Melt Flow
17.5
g/10 min
@Load 1.20 kg,
Temperature 300 °C
17.5
g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
66.0
MPa
9570
psi
50 mm/min; ASTM D638
Tensile Strength, Yield
63.0
MPa
9140
psi
50 mm/min; ASTM D638
Elongation at Break
120 %
120 %
50 mm/min; ASTM D638
Elongation at Yield
7.0 %
7.0 %
50 mm/min; ASTM D638
Flexural Yield Strength
100
MPa
14500
psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
2.35
GPa
341
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched
8.20
J/cm
15.4
ft-lb/in
ASTM D256
2.00
J/cm
@Temperature -30.0 °C
3.75
ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched
21.4
J/cm
40.1
ft-lb/in
ASTM D4812
Dart Drop, Total Energy
77.0
J
56.8
ft-lb
ASTM D3763
Falling Dart Impact
169
J
125
ft-lb
ASTM D3029
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
63.6
µm/m-°C
@Temperature -40.0 - 40.0 °C
35.3
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow
65.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
36.1
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Specific Heat Capacity
1.26
J/g-°C
0.301
BTU/lb-°F
ASTM C 351
Thermal Conductivity
0.190
W/m-K
1.32
BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi)
137
°C
@Thickness 3.20 mm
279
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
132
°C
@Thickness 3.20 mm
270
°F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point
143
°C
289
°F
Rate B/50; ASTM D1525
Optical Properties
Metric
English
Comments
Refractive Index
1.586
1.586
ASTM D542
Haze
1.0 %
@Thickness 2.54 mm
1.0 %
@Thickness 0.100 in
ASTM D1003
Transmission, Visible
88 %
@Thickness 2.54 mm
88 %
@Thickness 0.100 in
ASTM D1003
Processing Properties
Metric
English
Comments
Nozzle Temperature
275
-
300
°C
527
-
572
°F
Injection Molding
Zone 1
260
-
280
°C
500
-
536
°F
Zone 2
270
-
295
°C
518
-
563
°F
Zone 3
280
-
305
°C
536
-
581
°F
Melt Temperature
280
-
305
°C
536
-
581
°F
Mold Temperature
70.0
-
95.0
°C
158
-
203
°F
Drying Temperature
120
°C
248
°F
Injection Molding
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Injection Molding
48.0
hour
48.0
hour
Cumulative; Injection Molding
Moisture Content
0.020 %
0.020 %
Back Pressure
0.300
-
0.700
MPa
43.5
-
102
psi
Shot Size
40 - 60 %
40 - 60 %
Vent Depth
0.00250
-
0.00760
cm
0.000984
-
0.00299
in
Screw Speed
40
-
70
rpm
40
-
70
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABI10387 / 243854
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.