MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Fusabond® M603 Polymer Modifier
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Fusabond® M603 Resin is a random ethylene copolymer, incorporating a monomer which is classified as being a maleic anhydride equivalent for application uses.

Fusabond® M603 is used in a variety of applications where adhesion improvements are needed for coatings, or compatibilization is need for compounds. In these applications, the Fusabond® resin is typically dry blended with a polyolefin matrix polymer for further processing. Examples include: Adhesives, Polymer Modification, Wood-Plastic Composites.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792, ISO 1183
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 108 °C226 °FASTM D3418, ISO 3146
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 260 °C<= 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema OREVAC® 18707 Grafted Maleic Anhydride Polypropylene
Dow Fusabond® E226 Polymer Modifier
Dow Fusabond® P613 Polymer Modifier
Dow Fusabond® C190 Polymer Modifier
Dow Fusabond® E265 Polymer Modifier

PDTA4956 / 170396

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.