MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Lead Alloy
Categories: Metal; Nonferrous Metal; Lead Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Lead Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.34 - 11.7 g/ccAverage value: 10.5 g/cc Grade Count:419
Thickness 102 - 173 micronsAverage value: 141 microns Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 3.00 - 33.0Average value: 11.8 Grade Count:64
Tensile Strength, Ultimate 12.0 - 317 MPaAverage value: 39.0 MPa Grade Count:136
Tensile Strength, Yield 6.00 - 66.0 MPaAverage value: 31.3 MPa Grade Count:9
Elongation at Break 2.00 - 101 %Average value: 33.0 % Grade Count:78
Modulus of Elasticity 13.8 - 36.4 GPaAverage value: 18.4 GPa Grade Count:32
Poissons Ratio 0.380 - 0.420Average value: 0.400 Grade Count:3
Shear Modulus 4.90 - 12.0 GPaAverage value: 9.30 GPa Grade Count:3
Shear Strength 12.4 - 52.0 MPaAverage value: 26.3 MPa Grade Count:22
Adhesive Bond Strength 19.5 - 30.0 MPaAverage value: 23.6 MPa Grade Count:5
Peel Strength 0.340 - 0.548 kN/mAverage value: 0.455 kN/m Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000140 - 0.0000905 ohm-cmAverage value: 0.0000246 ohm-cm Grade Count:86
Magnetic Susceptibility -1.20e-7Average value: -1.20e-7 Grade Count:4
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.6 - 30.4 µm/m-°CAverage value: 26.5 µm/m-°C Grade Count:104
Specific Heat Capacity 0.100 - 0.197 J/g-°CAverage value: 0.136 J/g-°C Grade Count:30
Thermal Conductivity 15.0 - 58.0 W/m-KAverage value: 32.5 W/m-K Grade Count:77
Melting Point 47.0 - 579 °CAverage value: 238 °C Grade Count:187
Solidus 47.0 - 327 °CAverage value: 218 °C Grade Count:171
Liquidus 47.0 - 579 °CAverage value: 251 °C Grade Count:170
Boiling Point 1750 °CAverage value: 1750 °C Grade Count:7
Maximum Service Temperature, Air 82.0 - 121 °CAverage value: 104 °C Grade Count:4
Minimum Service Temperature, Air -51.0 - -18.0 °CAverage value: -38.5 °C Grade Count:4
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.630Average value: 0.630 Grade Count:3
Reflection Coefficient, Visible (0-1) 0.620Average value: 0.620 Grade Count:4
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.00100 - 0.0300 %Average value: 0.00619 % Grade Count:64
Antimony, Sb 0.000500 - 29.0 %Average value: 5.07 % Grade Count:207
Arsenic, As 0.000500 - 3.00 %Average value: 0.264 % Grade Count:93
As + Sb + Sn 0.00200 %Average value: 0.00200 % Grade Count:6
Barium, Ba 0.0500 - 2.00 %Average value: 0.491 % Grade Count:11
Bismuth, Bi 0.00500 - 55.5 %Average value: 6.67 % Grade Count:102
Cadmium, Cd 0.000500 - 17.0 %Average value: 1.03 % Grade Count:37
Calcium, Ca 0.00800 - 6.00 %Average value: 0.376 % Grade Count:41
Copper, Cu 0.000500 - 55.0 %Average value: 1.21 % Grade Count:92
Indium, In 1.00 - 60.0 %Average value: 21.1 % Grade Count:40
Iron, Fe 0.000500 - 0.350 %Average value: 0.0323 % Grade Count:68
Lead, Pb 22.6 - 100 %Average value: 81.7 % Grade Count:448
Lithium, Li 0.0100 - 0.700 %Average value: 0.151 % Grade Count:14
Nickel, Ni 0.000500 %Average value: 0.000500 % Grade Count:4
Selenium, Se 0.0200 %Average value: 0.0200 % Grade Count:3
Silver, Ag 0.000100 - 40.0 %Average value: 2.32 % Grade Count:90
Strontium, Sr 0.0600 - 2.00 %Average value: 0.605 % Grade Count:4
Sulfur, S 0.00100 - 0.500 %Average value: 0.0359 % Grade Count:16
Tellurium, Te 0.0350 - 0.0600 %Average value: 0.0419 % Grade Count:4
Tin, Sn 0.000500 - 63.0 %Average value: 17.3 % Grade Count:304
Zinc, Zn 0.000500 - 0.0100 %Average value: 0.00463 % Grade Count:72

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nickel Alloy
Overview of materials for Copper Alloy
Overview of materials for Molybdenum Alloy
Overview of materials for Tin Alloy
Lead, Pb

M01058 / 81671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.