MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ovako 18CrNiMo7-6 159Q Steel, Hardening
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel

Material Notes: General Information: 18CrNiMo7-6 is a case hardening steel with high toughness. There are a number of variants with high cleanliness requirements. All variants possess tighter composition ranges compared to the standard. One variant is produced with the quality class IQ (isotropic quality). This ensures a very low number of elongated sulphide inclusions which will give more isotropic properties. The high oxidic cleanliness will enable the steel to meet the same high cleanliness demands as for re-melted qualities.
Grade 159A - Variant with low sulphur content and high cleanliness demands
Grade 159B - Variant with controlled sulphur content for consistent machinability and +H hardenability
Grade 159Q - Isotropic properties (IQ) and better fatigue strength due to higher cleanliness levels, and a finer size and distribution of non-metallic inclusions
Grade 159X - Variant with controlled sulphur content for consistent machinability and +H hardenability
Grade 159S - Variant with increased sulphur content.
Grade 4761(MoCN216) - Low sulphur variant of ImatraIQ-SteelIQ-Steel® is an isotropic quality ultra clean steel optimized for high fatigue strength under multi axial loading.

Information provided by Ovako

Key Words: 1.6587, AISI4820, DIN17CrNiMo6, 18CND6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  980 - 1270 MPa
@Thickness 63.0 mm
142000 - 184000 psi
@Thickness 2.48 in
 1080 - 1320 MPa
@Thickness 30.0 mm
157000 - 191000 psi
@Thickness 1.18 in
Tensile Strength, Yield  >= 690 MPa
@Thickness 63.0 mm
>= 100000 psi
@Thickness 2.48 in
 >= 780 MPa
@Thickness 30.0 mm
>= 113000 psi
@Thickness 1.18 in
Elongation at Break  8.0 %
@Thickness 30.0 mm
8.0 %
@Thickness 1.18 in
 8.0 %
@Thickness 63.0 mm
8.0 %
@Thickness 2.48 in
Modulus of Elasticity 210 GPa30500 ksi
Poissons Ratio 0.300.30
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
6.67 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
0.110 - 0.115 BTU/lb-°F
@Temperature 122 - 212 °F
Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
Transformation Temperature 410 °C770 °FMS
 726 °C1340 °FAC1
 833 °C1530 °FAC3
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.16 - 0.19 %0.16 - 0.19 %
Chromium, Cr 1.6 - 1.8 %1.6 - 1.8 %
Iron, Fe 94.99 - 95.79 %94.99 - 95.79 %As Balance
Manganese, Mn 0.50 - 0.60 %0.50 - 0.60 %
Molybdenum, Mo 0.25 - 0.35 %0.25 - 0.35 %
Nickel, Ni 1.5 - 1.7 %1.5 - 1.7 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si 0.20 - 0.35 %0.20 - 0.35 %
Sulfur, S <= 0.0020 %<= 0.0020 %
 
Descriptive Properties
WeldabilityCEV 0.86max
 Pcm 0.39max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ovako 18CrNiMo7-6 159A Steel, Hardening
Ovako 18CrNiMo7-6 159S Steel, Hardening
Ovako 18CrNiMo7-6 4761 MbCN 216 Steel, +AR
Ovako 18CrNiMo7-6 ref Steel
Ovako 18CrNiMo7-6 4761 MbCN 216 Steel, +A

NOVAKO102 / 234401

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.